top of page

SMCO SINTERED MAGNET
Low temperature coefficient - Suitable for cryogenic applications

YX Magnetic SA's SmCo magnets, an alloy of samarium and cobalt, are distinguished by their high magnetism and thermal stability.

 

YX MAGNETIC SA offers:

  • Block Dimensions : Up to 130mm x 80mm x 50mm, with full saturation.

  • High Quality Mass Production : Specialized in YXG-33H magnets with a (BH)max of 30-33MGOe.

  • Precise Magnetic Alignment : Less than 3 degrees of deviation, for perfect consistency.

  • Advanced Sm1Co5 Manufacturing : Capable of mass producing multi-pole planar magnets with less than 6mm magnetization thickness.

Permanent magnet - SmCo magnet - irregular Magnet
Production process

Magnet SmCo1:5

SmCo1-5 Magnet
  1. The maximum range (BH) is 16 to 25 MGOe, the maximum working temperature is 250oC.

  2. The physical characteristics and ductility of SmCo5 are better than those of Sm2Co17. This makes Smco5 slightly easier to machine. 

  3. Compared to the magnetic field, SmCo5 is lower than Sm2Co17, a magnetic field of 40,000 gauss can be saturated.

Sm2Co17

Sm2Co17
  1. The maximum range (BH) is 20 to 35MGOe. The maximum working temperature is 350oC.

  2. Sm2Co17 has an extremely low temperature coefficient and preferably anti-causticity. 

  3. There is no need to coat it because it is difficult to erode and oxidize.

Sintered Samarium Cobalt (SM1CO5/SM2CO17) magnets Catalog

Click link to download the full version.

  1. Further qualities or grade on low thermal coefficient magnets, please contact us for more details. 

  2. The maximum operating temperature depends on the magnet's dimensions and its final applications. We recommend keeping a margin of safety in materials selection.

bottom of page